Sunday, 22 November 2026

7 Purlin Roll Forming Defects: Causes and On-Line Fixes

Why Defects Start Upstream, Not at the Shear

Purlin roll forming defects rarely start at the shear. They start stands upstream, where a strip meets a roll gap that is too tight or a web that is off centre. By the time a part leaves the line, twist, bow or a hole out of position looks like one fault. It is usually seven faults with seven fixes.

The Seven Defects and What Each Traces To

The seven are twist, longitudinal bow, springback, edge wave, end flare, hole position drift and surface galling. Each traces to one variable: roll gap, stand alignment, overbend angle, finishing reduction, shear clearance, encoder sync or roll surface. A defect is a measurement, not an impression, so group it by type before touching the machine.

Geometric Defects: Twist, Bow and Springback

Twist comes from a roll gap that differs across the web or stands not square to the pass line. Balance the gaps and add a straightening head with side roll adjustment, then hold rise under 2 mm over 1 m. Bow follows the coil: the entry guide, pinch roll and first stand must share one line, because a guide 2 mm out at the entry can become 20 mm of sweep over 6 m. Springback rises with yield strength, so a 550 MPa section opens more than a 345 MPa one. Controlled overbend keeps it within ±2 degrees of the drawing.

Surface and Position Defects

Edge wave comes from too much reduction in the finishing passes, which stretches the edge more than the web. Ease closing pressure on the last two stands. Galling means zinc or scale has welded to a roll surface, so clean the roll and restore lubricant flow. Hole drift is the most costly defect: the encoder and punch frame must agree, and each hole should land within ±0.5 mm on a 6 m part. End flare opens in the first 100 mm of a cut part, so use a sharp shear at clearance near 10 percent of thickness.

Record the Numbers at FAT

Run your own coil at three settings and measure a part each time. The acceptance targets, twist under 2 mm per 1 m, bow under 3 mm over 6 m, holes within ±0.5 mm, turn seven fixes into evidence you can hold a supplier to.

Read the full article →

No comments:

Post a Comment

7 Purlin Roll Forming Defects: Causes and On-Line Fixes

Why Defects Start Upstream, Not at the Shear Purlin roll forming defects rarely start at the shear. They start stands upstream, where a str...