Cellular Floor Deck Roll Forming: 6 Double-Line Techniques

Two Coils Set the Whole Line

Cellular production starts with developed strip width, not tonnage. The deck coil must yield the rib geometry, the side laps and the embossments. The pan coil must match the finished coverage minus the lap. Typical deck depths are 1.5, 2.0 and 3.0 in (38, 51 and 76 mm), with coverage of 24 or 36 in. Most deck runs G90 galvanized to ASTM A653, and the zinc layer is what the electrode sees first.

Split the Forming Train, Not the Frame

The deck train does the real work. A 3 inch profile needs 20 to 26 stands with 95 to 120 mm shafts. The pan train levels, edge forms and adds a slight crown, using 6 to 10 stands. Do not tie the two trains to one drive shaft, because different pass counts and different strip elongation force one of them to slip. Two frames, two gearboxes and one control cabinet is the arrangement that survives multi-shift running.

Sync at the Register

Speed matching is an encoder problem. The deck line carries the master encoder and the pan line follows through a dancer loop. Registration happens about 1 m before the first weld head, with a target of ±1 mm. Beyond 1.5 mm the nugget sits off centre and the cell opens under load.

Weld Pitch Caps the Line Speed

A typical schedule uses stitch welds at 12 in (305 mm) pitch with a nugget of at least 4.8 mm, and output settles at 15 to 25 m/min even when both trains can run 40 m/min. Change current and force with the gauge pair, and dress the electrodes every shift.

Read the full article →

Deep Deck vs Shallow Deck Roll Forming: 7 Tooling Comparisons

Stand Count and Bend Angle Per Pass

Stand count is the first number that separates a shallow deck line from a deep one. A 38 mm shallow profile forms cleanly in 14 to 18 stands. A 76 mm deep profile needs 24 to 30, and a 100 to 125 mm section pushes that to 30 to 36. Keep each pass to about 10 to 15 degrees at the rib root, because a taller rib formed in too few stands asks for 25 degrees or more per pass and the outside of the bend starts to thin.

Shafts, Stands and Roll Blanks

Deep ribs load the frame harder. Forming force at the rib root runs two to three times the shallow figure, and torque per stand climbs from 1.5 to 2.5 kN·m to 4 to 8 kN·m. Shafts grow from 60 to 75 mm to 80 to 100 mm, and stand plates from 35 to 45 mm to 55 to 70 mm. Roll blanks go from 180 to 260 mm to 260 to 360 mm, easing the contact angle at the rib root.

Drive Power and Line Speed

A shallow line runs one motor and a geared distribution shaft. A deep line splits into two drive groups. Drive power rises from 30 to 45 kW to 75 to 110 kW, and line speed drops from 25 to 40 m/min to 12 to 25 m/min. Speed is the trade buyers notice first, because the cutoff die clears a taller rib and the embossment rolls need dwell time.

The Cutoff Stroke

A flying shear needs a stroke equal to rib depth plus 20 to 30 mm. A 38 mm profile clears in 60 mm, a 125 mm profile in 150 mm. That means a heavier shear, a longer servo cycle and a slower line. Do not quote a deep line at shallow line rates.

Read the full article →

Cellular Floor Deck Roll Forming: 6 Double-Line Techniques

Two Coils Set the Whole Line Cellular production starts with developed strip width, not tonnage. The deck coil must yield the rib geometry,...