Showing posts with label quality control. Show all posts
Showing posts with label quality control. Show all posts

Sunday, 22 November 2026

Coating Peeling in Roll Forming: 7 Root Causes From Coil to Panel

Why a Coating That Passes on Flat Sheet Peels at the Roll

Adhesion tests on flat sheet measure a bond at zero strain. Roll forming does not run at zero strain. At the outer radius of a bend, the steel elongates and the film bonded to it must elongate by the same amount. On a tight rib that strain reaches 10 to 20 percent, applied in a fraction of a second. That gap explains why a coil that passes a cross-hatch test at 5B and a T-bend at 1T can still show paint lifting at the rib corner.

Read the Failure Surface First

What sits under the flake tells you which interface failed. Bare grey steel with no zinc points to pretreatment or primer to substrate. Bright zinc with no primer residue points to primer cure. Primer on the steel with topcoat on the flake points to the intercoat. Lifted along one side points to friction at the roll face, and lifted from a cut edge points to shear burr or edge damage.

The Coil and the Coating System

Polyester topcoats cure to a peak metal temperature of 232 to 243 C, with primers lower, around 204 to 232 C. If the primer never reached its PMT, the film stays under-crosslinked and fails under forming stress even though a flat coupon passes. Over-cure embrittles the film, and a line stop with strip sitting in the oven does the same.

The Bend Radius and the Line

A 1.5 mm sheet bent to a 1.5 mm inside radius puts roughly 33 percent strain on the outer film, and no standard architectural coating survives that. Then the line can add its own damage. A roll gap set too tight turns forming into a compression test, and a rough roll face drags the film. Set gap by thickness plus 5 to 10 percent per side.

Read the full article →

Roll Forming Lubrication: 6 Rules for Clean, Stable Surfaces

What the Film Actually Does

A roll forming lubricant does five jobs at once: it lowers friction, carries heat out of the forming zone, flushes metal fines, leaves a temporary corrosion barrier and extends roll and punch life. Heat is the function most plants ignore. A mill running 30 m/min without coolant can lift strip temperature by 20 to 40 C from entry to last stand, and that heat thins the film where strain is highest.

Match the Chemistry to the Surface

Cold rolled and hot rolled steel are inactive surfaces and accept most ferrous lubricants. Galvanized and Galvalume stock can stain and start white rust with aggressive extreme pressure additives. Aluminium darkens above pH 9. Prepainted coil loses paint, adhesive and weld bond under silicone or heavy wax. A compatibility test is cheap: soak three coupons in the candidate lubricant for 24 hours at 40 C.

Set Film Weight, Not a Squirt

Film weight is the only number that makes lubrication repeatable. A vanishing oil on prepainted panel runs at 0.3 to 0.5 g/m². General galvanized and cold rolled work sits at 0.8 to 2 g/m². Heavy gauge or tight radius work needs 2 to 5 g/m². A metered roller coater holds about plus or minus 10 percent.

Clean Strip Beats Extra Oil

A 50 µm particle trapped between roll and strip leaves a scratch 5 to 20 µm deep. A 25 µm absolute filter on the recirculation loop removes most of the load, while a 100 µm strainer is a chip guard, not a filter. Wiper felts at the entry and after the applicator spread the film and wipe the back face.

Read the full article →

First Article Inspection in Roll Forming: 6 Checks Before Sign-Off

Why First Article Inspection Is Different

A first article inspection record is a one time dimension verification, not a running quality log. Inline inspection watches the line while it runs, while the first article record freezes one setup and attaches a signature to it. It asks one question: does the first good part match the drawing, and can the recipe be locked?

Prepare the Drawing, Coil and Samples

Review the drawing and assign balloon numbers, usually 8 to 14 characteristics with a nominal and tolerance beside each. Read the coil certificate and measure strip thickness at three points, treating a band such as 1.48 to 1.52 mm as an input, because roll gap and inside radius depend on it. Then cut and label three samples from the start, middle and end of the coil, since the three reveal drift a single piece would hide.

Record the Dimensions

Measure web width, flange height, bend angle and inside radius, such as an 80.0 mm web and a 1.5 mm inside radius. The inside radius sets section strength and coating strain at the corner. Then record cut length and hole position, such as 6000 mm within plus or minus 2 mm and a hole 250 mm from the leading edge within plus or minus 1 mm.

Surface, Sign-Off and Recipe Freeze

Inspect all three samples under good light for scratches, cracks, peeling and roll marks. Write the acceptance result, the sign-off name and date, and lock the recipe values for roll gap, line speed and overbend. The sign-off turns readings into a released setup, and it happens only after the three coil positions agree.

Read the full article →

Roll Forming Profile Measurement: 7 Methods Compared

What Profile Measurement Has to Capture

Roll forming profile measurement starts with the drawing. A cold formed section carries five or six critical dimensions set by the drawing, the roll tooling and the cutoff trigger. A 0.4 to 3.0 mm coil can drift by tenths of a millimetre. Tolerances are not universal: a steel deck profile to SDI criteria may allow a width band near 1.5 mm on a 300 mm section, while a trim to EN 10162 can be tighter.

Seven Methods Compared

A laser profile scanner reads a full 2D section in 2 to 10 seconds at 0.02 to 0.05 mm. An optical comparator reads bend angle and inside radius in 1 to 3 minutes. A CMM is the most accurate at 0.005 to 0.02 mm but takes 5 to 20 minutes per part. A digital caliper and a radius gauge handle floor checks, a go/no-go fixture screens one dimension in 1 to 3 seconds, and a line-mounted laser reads a moving strip at 0.05 to 0.2 mm.

Where to Sample a Coil

A coil is not uniform end to end. The head carries the setup transient and the tail carries coil crown and changing tension. Take samples at the start, middle and end of every coil, keep three parts from the head and three from the tail, and log the metre mark on each. A common plan takes 2 parts per 1000 m of steady run.

Springback and Temperature

A 90 degree corner does not stay at 90 degrees. Mild steel springs back 1 to 3 degrees and HSLA grades 3 to 6 degrees. Steel also grows about 0.012 mm per metre per degree Celsius, so let the sample reach 20 degrees Celsius before you log data.

Read the full article →

Cellular Floor Deck Roll Forming: 6 Double-Line Techniques

Two Coils Set the Whole Line Cellular production starts with developed strip width, not tonnage. The deck coil must yield the rib geometry,...