Sunday, 22 November 2026

Cellular Floor Deck Roll Forming: 6 Double-Line Techniques

Two Coils Set the Whole Line

Cellular production starts with developed strip width, not tonnage. The deck coil must yield the rib geometry, the side laps and the embossments. The pan coil must match the finished coverage minus the lap. Typical deck depths are 1.5, 2.0 and 3.0 in (38, 51 and 76 mm), with coverage of 24 or 36 in. Most deck runs G90 galvanized to ASTM A653, and the zinc layer is what the electrode sees first.

Split the Forming Train, Not the Frame

The deck train does the real work. A 3 inch profile needs 20 to 26 stands with 95 to 120 mm shafts. The pan train levels, edge forms and adds a slight crown, using 6 to 10 stands. Do not tie the two trains to one drive shaft, because different pass counts and different strip elongation force one of them to slip. Two frames, two gearboxes and one control cabinet is the arrangement that survives multi-shift running.

Sync at the Register

Speed matching is an encoder problem. The deck line carries the master encoder and the pan line follows through a dancer loop. Registration happens about 1 m before the first weld head, with a target of ±1 mm. Beyond 1.5 mm the nugget sits off centre and the cell opens under load.

Weld Pitch Caps the Line Speed

A typical schedule uses stitch welds at 12 in (305 mm) pitch with a nugget of at least 4.8 mm, and output settles at 15 to 25 m/min even when both trains can run 40 m/min. Change current and force with the gauge pair, and dress the electrodes every shift.

Read the full article →

Cellular Floor Deck Roll Forming: 6 Double-Line Techniques

Two Coils Set the Whole Line Cellular production starts with developed strip width, not tonnage. The deck coil must yield the rib geometry,...